TECATRON PPS CM GF40 natural (XP64)
Modified PPS
This compression molded PPS material is modified with 40% glass fibers for increased strength and stiffness
Mechanical properties | Value | Unit | Condition | Test Method |
---|---|---|---|---|
Modulus of elasticity (flexural test) |
1,250,000 | psi | ASTM D 790 | |
Shore hardness | 90 | Shore D | ASTM D 2240 | |
Flexural strength | 13,000 | psi | @73°F | ASTM D 790 |
Elongation at break (tensile test) | 1.2 | % | ASTM D 638 | |
Tensile strength | 8,000 | psi | ASTM D 638 | |
Modulus of elasticity (tensile test) |
1,300,000 | psi | ASTM D 638 | |
Impact strength (Izod) | .5 | ftlbsin | ASTM D 256 | |
Compression strength | 21,000 | psi | @ 10% | ASTM D 695 |
Compression modulus | 650,000 | psi | ASTM D 695 | |
Compression strength | 8,000 | psi | @ 1% | ASTM D 695 |
Rockwell hardness | 82 | M Scale | ASTM D 785 |
Thermal properties | Value | Unit | Condition | Test Method |
---|---|---|---|---|
Heat distortion temperature | 234 | F | ASTM D 648 | |
Thermal expansion (CLTE) | 28*10-6 / | F | ASTM D 696 |
Electrical properties | Value | Unit | Condition | Test Method |
---|---|---|---|---|
Dielectric strength | 233 | V/mil | ASTM D 149 |
Other properties | Value | Unit | Condition | Test Method |
---|---|---|---|---|
Moisture absorption | .063 | % | @ 24 hrs | ASTM D 570 |