TECAPEEK CM XP96 natural
Unfilled PEEK
This compression molded material is an unfilled Victrex® PEEK polymer available in rods, tubes and plates.
Mechanical properties | Value | Unit | Condition | Test Method |
---|---|---|---|---|
Tensile strength at break | 15,000 | psi | @73°F | ASTM D 638 |
Elongation at break (tensile test) | 10 | % | @73°F | ASTM D 638 |
Modulus of elasticity (tensile test) |
700,000 | psi | @73°F | ASTM D 638 |
Flexural strength | 25,000 | psi | @73°F | ASTM D 790 |
Modulus of elasticity (flexural test) |
660,000 | psi | @73°F | ASTM D 790 |
Compression strength | 19,300 | psi | @73°F, 10% strain | ASTM D 695 |
Compression modulus | 360,000 | psi | @73°F | ASTM D 695 |
Impact strength (Izod) | .58 | ftlbsin | @73°F, notched | ASTM D 256 |
Shore hardness | 88 | D Scale | ASTM D 2240 | |
Elongation at yield (tensile test) | 6.7 | % | ASTM D 638 |
Thermal properties | Value | Unit | Condition | Test Method |
---|---|---|---|---|
Deflection temperature | 300 | F | ASTM D 648 | |
Thermal conductivity | 1.7 | BTU-in/hr-ft^2 - deg | ASTM C 177 | |
Melting temperature | 649 | F | - | |
Service temperature | 500 | F | Short Term | - |
Electrical properties | Value | Unit | Condition | Test Method |
---|---|---|---|---|
Dielectric strength | 1900 | kV/mm | ASTM D 149 | |
volume resistance | 4.9*1016 | Ω*cm | ASTM D 257 |
Other properties | Value | Unit | Condition | Test Method |
---|---|---|---|---|
Moisture absorption | 0.05 | % | ASTM D 570 |