TECATRON PPS CM XP64 natural
modified PPS
This compression molded PPS material is modified with 40% glass fibres for increased strength and stiffness.
>
Mechanical properties | Value | Unit | Parameter | Norm |
---|---|---|---|---|
Modulus of elasticity (tensile test) |
6200 | MPa | ASTM D 638 | |
Tensile strength | 42 | MPa | ASTM D 638 | |
Elongation at break (tensile test) | 1.1 | % | ASTM D 638 | |
Flexural strength | 75 | MPa | ASTM D 790 | |
Modulus of elasticity (flexural test) |
8200 | MPa | ASTM D 790 | |
Compression modulus | 3900 | MPa | ASTM D 695 | |
Compression strength | 172 | MPa | ASTM D 695 | |
Shore hardness | 88 | - | Shore D | ASTM D 2240 |
Thermal properties | Value | Unit | Parameter | Norm |
---|---|---|---|---|
Heat distortion temperature | 112 | C | ASTM D 648 |